Under what conditions can spray welding be used?

author:admintime:2019-09-22 22:20click:
            Spray welding is to reheat the preheated self-soluble alloy powder coating to 1000-1300 C, melt the particles, float the slag onto the surface of the coating, and disperse the boride and silicide in the coating, so as to achieve good bonding between the particles and the surface of the substrate.
            Spray welding process is suitable for the following situations:
            1. Surface loads of various kinds of carbon and low alloy steels are large, especially those subjected to impact loads. For workpieces with bonding strength of 350-450N/mm2, spray welding hardness HRC150 < 65, coating thickness from 0.3 to several millimetres, and surface roughness of spray welding layer after grinding can reach Ra0.4-0.1 micrometres.
            2. When used in corrosive media, the coating is required to be compact and porous.
            3. Hardening, carburizing, nitriding and hard chromium plating are used in the original design of workpiece surface, which requires high hardness.
            4. Workpiece working environment is bad, such as strong abrasive wear, erosion wear, cavitation and so on.
            5. Oxygen-acetylene flame alloy powder spray welding process is suitable for surface strengthening or repairing of various carbon steel and low alloy steel parts, but some characteristics of parts material should be noticed. When the linear expansion coefficient of matrix material differs greatly from that of alloy spray welding layer, it should be used cautiously when the linear expansion coefficient of matrix material is less than 12 *10-6/~C and more than 12 *10-6/~C, so as to avoid manufacturing. Cracks can also be difficult to spray welding if the content of elements with high affinity to oxygen in matrix metals is more than 3%, the total content of elements such as tungsten and molybdenum is more than 0.5%, or the sulfur content in steel is more than 0.5%. This is because these materials are easy to form dense and stable oxide film by interaction with oxygen to prevent melting. The wetting effect of the alloy on the matrix will cause the liquid alloy to roll like a "sweat bead" during remelting. Therefore, the adaptability of the spray welding process to the sprayed matrix material should be paid attention to.
            6. Metal materials that can be sprayed without special treatment:
            7. Metal materials that need to be preheated at 250-375 C after spray welding need to be slowly cooled.
            8. Metal materials requiring isothermal annealing after spray welding

Telephone

0769-85415700

function

Price

quality

service

Wechat sweep

Mobile phone sweep

软萌小仙自慰喷白浆| 好屌草这里只有精品| 日本50岁丰满熟妇xxxx| 亚洲狠狠色丁香婷婷综合| 成年女人免费视频播放体验区 | 国产精品视频一区无码| 成本人片无码中文字幕免费| 女性自慰网站免费观看| 麻豆人妻无码性色av专区| 精品一区二区三区AV天堂| 人妻乳哺乳无码一区二区| 久久99热这里只有精品国产| 久久国产精品久久久久久| 国产精品无码av无码| 巨大巨粗巨长 黑人长吊| 日本熟妇中文字幕三级| 国产亚洲欧美精品一区| 玩中年熟妇让你爽视频| 亚洲色精品vr一区二区三区| 亚洲精品TV久久久久久久久久 | √最新版天堂资源网在线| 亚洲av成人片色在线观看高潮| 无码少妇一区二区三区芒果| 国产精品特级毛片一区二区三区| 国内丰满熟女出轨VIDEOS| 婷婷久久综合九色综合绿巨人 | 护士人妻HD中文字幕| 亚洲av成人无码网站天堂网久久| 夜夜爽一区二区三区精品| 天天综合亚洲色在线精品| 7777久久亚洲中文字幕蜜桃| 黄 色 网 站 成 人免费| 欧美成人精品三级网站| 国产午夜精品一区二区三区软件| 最近中文字幕2018| 久久综合国产乱子伦精品免费| 人妻少妇久久久久久97人妻| 亚洲综合无码久久精品综合| 亚洲人成77777在线播放网站不卡| 国产精品igao视频网| 国产av无码专区亚洲av男同|